42 crmoa mechanical properties and chemical composition Mechanical properties Tensile strength σ b (MPa) : 1080 (110) or Yield strength σ s (MPa) : 930 (95) or Elongation δ 5 (%) : 12 or more Reduction of area ψ (%) : was 45 Impact work Akv (J) : 63 or more Impact toughness value α kv (J/cm2) : was 78 (8) Hardness: acuities 217 hb Sample size: sample blank dimensions to 25 mm [2] : (quenching 850 degrees; cooling agent: oil; tempering temperature 560 degrees; cooling agent: water, oil); Mechanics performance, tensile strength MPa1080, yield point MPa930, elongation % 12, reduction of area % 45, shock absorption Work Ak63, steel annealing or high temperature tempering supply state brinell hardness HBW acuities were 217; use Used for more than 35 crmo steel demand higher strength or section more forgings, such as locomotive traction wheel, supercharger drive tooth Wheel, axle, engine cylinder, 1200 ~ 2000 m deep petroleum well drill pipe joint and fishing tools, can replace contain Nickel higher quenched and tempered steel. The corresponding international standards organization brand: 42 crmo4 Corresponding Japanese brand: SCM440 Corresponding German brand: 42 crmo4 or 1.7225 Approximate corresponding American brand: 4140 or G41400 Chemical composition C0.38 ~ 0.45, Si0.17 ~ 0.37, Mn0.50 ~ 0.80, Cr0.90 ~ 1.20, Mo0.15 ~ 0.25
|